Inconel 800 steel coils have a density of approximately 8.0 g/cm³, a melting point between 1350℃ and 1400℃, and a coefficient of thermal expansion of 18×10⁻⁶/℃ in the range of 20℃ to 800℃. Its thermal conductivity is relatively low, 11.6 W/(m·K) at 20℃, increasing to 18.6 W/(m·K) at 600℃, and its electrical resistivity is 109 μΩ·cm at room temperature.
The elastic modulus of Inconel 800 alloy is 206 GPa, and its Poisson's ratio is 0.3. These physical properties allow it to effectively manage heat and maintain structural stability in high-temperature environments, making it suitable for industrial applications requiring high-temperature resistance and thermal shock resistance.